椰殼黃金炭
椰殼黃金炭主要用于炭漿法提取黃金及其它貴重金屬的提取。低口礦,高得率回收黃金,是金礦理想的活性炭。
優(yōu)適椰子殼黃金活性炭是以東南亞椰殼為原料,采用物理法及高溫水蒸氣活化工藝精制而成。黃金用活性炭顆粒度均勻,機(jī)械強(qiáng)度高,吸附力強(qiáng),后處經(jīng)水磨等特殊工藝制造而成,具有耐磨強(qiáng)度好、吸附性能高等特點(diǎn),適用于現(xiàn)代化金礦采金生產(chǎn),主要用于堆浸法或炭漿法提取黃金冶金工業(yè)中貴金屬的分離和提取。
黃金提取活性炭經(jīng)系列生產(chǎn)工藝精加工而成。外觀為黑色,呈顆粒狀,具有空隙發(fā)達(dá)、吸附性能好、強(qiáng)度高、易再生、經(jīng)濟(jì)耐用等優(yōu)點(diǎn)。椰殼黃金提取活性炭也可用于飲用水、凈水、制酒、飲料、工業(yè)污水的凈化、脫色、脫氯、除臭;也可用于煉油行業(yè)的脫硫醇等。
eishi ningbo coconut shell activated carbon activated carbon plant Description:
The products have developed pore structure, huge specific surface area, strong adsorptive properties and high intensity, widely used in treatment of kinds of water and extracting gold. They are used for decolorizing and reefing of monosodium, citric acid and wine, grease and oil.
The nut granular activated carbons are refined through carbonization and activation with apricot nutshell as raw material
椰殼黃金活性炭技術(shù)參數(shù):
粒 徑: 0.4-3mm
真 比 重: 2-2.2g/cm3
苯粉吸附率: ≥450mg/g
堆 比 重: 0.45-0.55g/cm3
強(qiáng) 度: ≥80-95%
總 孔 容積: 0.7-1cm3/g
碘 值: 1000-1100mg/g
比 表 面積: 590-1500m2/g
亞 甲 蘭值: 100-150mg/cm3
PH 值: 8-10
半 脫 氯值: ≤5cm
灰 份: ≤8-12%
水 份: ≤3%
比 熱: -1.00J/g.℃